Atomic layer deposition (ALD) for particle nanostructuring: achieving atomic precision in scalable nanofabrication schemes.

van Ommen, J. R. (Speaker), Aris Goulas (Speaker)

Activity: Talk or presentationTalk or presentation at a workshop, seminar, course or other meeting

Period2014
Event title12th Int. Conf. on Nanosciences and Nanotechnologies NN14
Event typeOther