Atomic layer deposition of alumina on nanoparticles at ambient conditions: process and applications

Valdesueiro Gonzalez, D. (Speaker), van Ommen, R. (Speaker), Kreutzer, M. (Speaker), Meesters, G. M. H. (Speaker)

Activity: Talk or presentationTalk or presentation at a workshop, seminar, course or other meeting

Period2015
Event titleChemE Faculty Colloquium 2015