Low-temperature atomic layer deposition of crystalline platinum nanoclusters on graphene nanoplatelets using (mettylcyclopentadienyl)-trimethylplatinum and oxygen

van Ommen, J. R. (Speaker), Hao Bui (Speaker), Fabio Grillo (Speaker)

Activity: Talk or presentationTalk or presentation at a workshop, seminar, course or other meeting

Period2015 → …
Event titleAVS 62nd International symposium & exhibition
Event typeExhibition