Analytical relationships for nanoindentation-based estimation of mechanical properties of biomaterials

J Rauker, P Rahnamay Moshtagh, HH Weinans, AA Zadpoor

Research output: Contribution to journalArticleScientificpeer-review

7 Citations (Scopus)
Original languageEnglish
Pages (from-to)1-44
Number of pages44
JournalJournal of Mechanics in Medicine and Biology
Volume14
Issue number3
DOIs
Publication statusPublished - 2014