Atomic Layer Deposition of CuInS2 for Solar Cells

M Nanu, J Schoonman, D Ursutiu, A. Duta, APLM Goossens

    Research output: Contribution to journalArticleScientificpeer-review

    Original languageUndefined/Unknown
    Pages (from-to)113-121
    Number of pages9
    JournalRevista De Tratamente Termice Si Ingineria Suprafetelor
    Volume1
    Publication statusPublished - 2003

    Keywords

    • professional journal papers
    • Geen BTA classificatie