@inproceedings{1694bb9cf5034f55a59264b22f7952a9,
title = "Atomic layer deposition TiO2 photonic crystal waveguide of biosensors",
keywords = "Elektrotechniek, Techniek, conference contrib. refereed, Conf.proc. > 3 pag",
author = "E Jardinier and G Pandraud and HTM Pham and PJ French and PM Sarro",
year = "2009",
doi = "doi:10.1088/1742-6596/187/1/012043",
language = "Undefined/Unknown",
isbn = "1742-6596",
publisher = "IOP Publishing",
pages = "1--4",
editor = "s.n.",
booktitle = "IOP journal of physics;conference series",
note = "null ; Conference date: 15-09-2008 Through 21-09-2008",
}