Fluidized-bed atomic layer deposition reactor for the synthesis of core-shell nanoparticles
AP Didden, J Middelkoop, WFA Besling, D. Nanu, R van de Krol
Research output: Contribution to journal › Article › Scientific › peer-review
11
Citations
(Scopus)