Impact of the atomic layer deposition precursors diffusion on solid-state carbon nanotube based supercapacitors performances

Research output: Contribution to journalArticleScientificpeer-review

18 Citations (Scopus)
Original languageEnglish
Pages (from-to)1-11
Number of pages11
JournalNanotechnology
Volume26
Issue number6
DOIs
Publication statusPublished - 2015

Bibliographical note

Harvest
Published 20-1-2015

Cite this