Spark plasma sintering of Stellite®-6 superalloy

M. Kiani Khouzani, A. Bahrami, M. Yazdan Mehr

Research output: Contribution to journalArticleScientificpeer-review

5 Citations (Scopus)
10 Downloads (Pure)

Fingerprint Dive into the research topics of 'Spark plasma sintering of Stellite®-6 superalloy'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science