Stochastic approach to the spatial analysis of pitting corrosion and pit interaction

JM Lopez de la Cruz, RHA Lindelauf, L Koene, MA Gutierrez De La Merced

    Research output: Contribution to journalArticleScientificpeer-review

    13 Citations (Scopus)
    Original languageUndefined/Unknown
    Pages (from-to)325-330
    Number of pages6
    JournalElectrochemistry Communications
    Volume9
    Publication statusPublished - 2007