Fingerprint
Dive into the research topics of 'Thermal atomic layer deposition of gold nanoparticles: Controlled growth and size selection for photocatalysis'. Together they form a unique fingerprint.- Sort by
- Weight
- Alphabetically
Fatemeh S.M. Hashemi, Fabio Grillo, Vikram R. Ravikumar, Dominik Benz, Ankit Shekhar, Matthew B.E. Griffiths, Seán T. Barry, J. Ruud Van Ommen