Climb enabled discrete dislocation plasticity of superalloy

C Ayas, V. Deshpande

Research output: Chapter in Book/Conference proceedings/Edited volumeConference contributionScientificpeer-review

5 Citations (Scopus)
Original languageEnglish
Title of host publicationMaterial Forming - ESAFORM 2015
Subtitle of host publicationProceedings of the 18th International ESAFORM Conference on Material Forming
EditorsA. Ofenheimer, C. Poletti, D. Schalk-Kitting, C. Sommitsch
PublisherTrans Tech Publications
Pages981-986
ISBN (Print)978-3-03835-471-0
DOIs
Publication statusPublished - 2015
EventESAFORM 2015: 18th International ESAFORM Conference on Material Forming - Graz, Austria
Duration: 15 Apr 201517 Apr 2015

Publication series

Name
PublisherTrans Tech Publications
NameKey Engineering Materials
Volume651-653
ISSN (Print)1013-9826

Conference

ConferenceESAFORM 2015: 18th International ESAFORM Conference on Material Forming
CountryAustria
CityGraz
Period15/04/1517/04/15

Keywords

  • Discrete dislocations
  • climb
  • vacancy diffusion
  • plasticity
  • superalloys

Cite this