@inproceedings{924479490b6b4ff29c114e3062886917,
title = "The effects of environmental impacts on durability of laminated glass plates with interlayers (SG, EVA, PVB)",
abstract = "The durability of laminated glass is a relevant problem in modern structural engineering. This paper deals with the results of experiments on laminated glass durability focusing on the following impacts: temperature, humidity, UV radiation and combination of these impacts. The purpose of this research is to investigate the aspect of laminated glass durability in the framework of long-term tests. Three different interlayer laminates were used during the experiments: Polyvinyl butyral (PVB), Ethylene vinyl acetate (EVA), DuPont's SentryGlas ionoplast (SG) and 6 mm thick tempered Soda-Lime-Silica Glass. Tests for environmental condition impact and durability of laminated glass are foreseen according to standard (ISO 12543- 4:2011). Bending tests were carried out due to standard (EN 1288-3:2000). Brief graphical comparison of the experimental results is presented in the paper.",
author = "T. Serafinavicius and Lebet, {J. P.} and C. Louter and A. Kuranovas and T. Lenkimas",
year = "2014",
doi = "10.1201/b16499-66",
language = "English",
isbn = "9781138001640",
series = "Challenging Glass 4 and COST Action TU0905 Final Conference - Proceedings of the Challenging Glass 4 and Cost Action TU0905 Final Conference",
publisher = "CRC Press / Balkema - Taylor & Francis Group",
pages = "455--462",
booktitle = "Challenging Glass 4 and COST Action TU0905 Final Conference - Proceedings of the Challenging Glass 4 and Cost Action TU0905 Final Conference",
note = "Challenging Glass 4 and Cost Action TU0905 Final Conference ; Conference date: 06-02-2014 Through 07-02-2014",
}